Thermoplastic Polymers

PP Random Copolymer Injection Grade RM 85 84

CAS 9010-79-1

Generic registry number (not stated in the manufacturer TDS)

Polypropylene reactor random copolymer

At a glance
MFR (230 °C, 2.16 kg)
Typical: 85 g/10 min
Tensile stress at yield [2]
Typical: 29 MPa
Tensile strain at yield [2]
Typical: 11 %
Flexural modulus [2]
Typical: 1250 MPa

Technical Specifications

ParameterValueMethod / unit
AppearancePellets
MFR (230 °C, 2.16 kg)Typical: 85 g/10 minISO 1133-1 · °C
Tensile stress at yield [2]Typical: 29 MPaISO 527-1,2
Tensile strain at yield [2]Typical: 11 %ISO 527-1,2 · %
Flexural modulus [2]Typical: 1250 MPaISO 178
Izod impact strength (notched, 23 °C) [2]Typical: 3.5 kJ/m²ISO 180/A · °C
Haze [18]Typical: 7 %ISO 14782 · %
HDT (0.45 MPa, flatwise) [2]Typical: 79 °CISO 75-1,2 · °C
Recommended processing temperatureTypical: 220 – 240 °C°C

Detailed application areas

Thin wall injection moulding requiring high clarity and low haze: media boxes, food packages, cups, closures and household articles. Can be processed on standard injection moulding machines.

Packaging & storage

Packaging

25 kg PE bags; 1375 kg polymer on shrink- or stretch-wrapped pallets. Road or rail silo transport is also available.

Storage

Protect from UV radiation and temperatures above 40 °C.

Documents

Technical data sheet (TDS)

Review the recorded specifications, packaging and storage information.

Download technical data sheet (PDF) ↓

Safety & lot documents

Request the current SDS and the certificate of analysis (CoA) for the lot you are evaluating.

KORKİMYA supply assurance

Stock in Türkiye

Current availability is confirmed by product and lot with your quote.

KKDİK registered

Every catalog product is KKDİK registered for Türkiye.

CoA for every lot

Verify technical values against the lot's certificate of analysis.

TL invoicing

Turkish lira invoicing is available for domestic purchases.

Payment terms

Discuss terms for your quantity and supply plan when requesting a quote.

Request Sample

Sample

Leave your email. Our sales team will get in touch about a sample and the certificate of analysis.

Response time · 24 hours

Product Information

PP Random Copolymer Injection Grade RM 85 84 (CAS 9010-79-1) is an industrial product in the thermoplastic polymers category. Typical specifications: Appearance: Pellets; MFR (230 °C, 2.16 kg): Typical: 85 g/10 min; Tensile stress at yield [2]: Typical: 29 MPa. KORKİMYA supplies PP Random Copolymer Injection Grade RM 85 84 in 25 kg PE bags; 1375 kg polymer on shrink- or stretch-wrapped pallets. Road or rail silo transport is also available..

Polypropylene reactor random copolymer

CAS
9010-79-1
TN-VED Code
3902 30
Category
Thermoplastic Polymers

Synonyms

TATREN RM 85 84

Test Methods

ISO 1133-1 · ISO 527-1,2 · ISO 178 · ISO 180/A · ISO 14782 · ISO 75-1,2

Key features

Why this product?

  • Observe fire safety rules for combustible materials. Dry pellets before use if moisture condenses inside packaging.
  • Contains clarifying and antistatic agents. [2] ISO 294-1 injection specimens. [18] 1 mm wall; melt 230 °C, cooling water 30 °C, overall cycle 15 s.
  • Only REACH-compliant raw materials are used.

Related Products

Last updated: 11/10/2026

MSDS Available · Export Registered · korkimya.com

KORKİMYA Updates

New products, capacity news, and KORKİMYA announcements - straight to your inbox.

Be the first to hear about new hydrocarbon resin launches, certifications, and industry events. No spam.

By subscribing, you accept our Privacy Policy.

PP Random Copolymer Injection Grade RM 85 84